Polymer Property : Dielectric Strength = 2850 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 112 kV/mm
2850 kV/in
Saint-Gobain CHR® 2345-2 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
Dielectric Strength 112 kV/mm
2850 kV/in
Saint-Gobain CHR® K109 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
Dielectric Strength 112 kV/mm
2850 kV/in
Saint-Gobain CHR® K350 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..