Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 103 kV/mm | 2620 kV/in | |
Saint-Gobain CHR® 2275-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |