Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.4 kV/mm | 645 kV/in | ASTM D149 |
CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC) Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or wh.. |
|||
Dielectric Strength | 25.4 kV/mm | 645 kV/in | ASTM D149 |
Arlon 55276B028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data represents typical values for the production mate.. |