Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 236 kV/mm | 6000 kV/in | ASTM D-149 |
Saint-Gobain Norton® FEP Fluoropolymer Film Features/Benefits:Outstanding clarityOutstanding anti-stick release propertiesPerformance from -254°C (-425°F) to 205°C (400°F)Exceptional chemical resistance and electric propertiesComp.. |
|||
Dielectric Strength | 236 kV/mm | 6000 kV/in | ASTM D-149 |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2919 Fluoropolymer Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Dielectric Strength | 236 kV/mm | 5990 kV/in | Flat sheets in air placed between 1/4 in diameter brass electrodes with 0.8 mm (1/32 in) edge radius subjected to 60 cycles AC voltage at 600V/s rate of rise to the breakdown voltage.; ASTM D149-81 |
DuPont™ Kapton® 200KN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Excellent processability, CTE close to copper, and a moderately high modulus.General Kapton® information: Kapton® is synthesized by polymerizing an aromatic dianh.. |