Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 22.8 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 22.8 kV/mm
580 kV/in
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite
Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Owens Corning Glass Fiber Reinforced Acetal, 25 wt.% glass
Data provided by the manufacturer, Owens Corning.
Dielectric Strength 22.8 kV/mm
580 kV/in
Short Term; ASTM D149
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet)
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow
Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow
Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow
Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Dielectric Strength 22.8 kV/mm
580 kV/in
Method A (Short-time); ASTM D149
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer  (discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Dielectric Strength 22.8 kV/mm
580 kV/in
ASTM D149
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples...
Dielectric Strength 22.8 kV/mm

@Thickness 2.00 mm
579 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL WCA875 PPE-TPE
Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t..
Dielectric Strength 22.8 kV/mm

@Thickness 2.00 mm
579 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Asia Pacific)
Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t..
Dielectric Strength 22.8 kV/mm

@Thickness 2.00 mm
579 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Europe-Africa-Middle East)
Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t..
Dielectric Strength 22.8 kV/mm
580 kV/in
Method A (Short-Time); ASTM D149
Techmer ES HiFill® PEEK GF30 HF 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc.
Dielectric Strength 22.8 kV/mm
580 kV/in
short time 2 mm thick; ASTM D149
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide
Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide ..
Copyright © lookpolymers.com All Rights Reserved