Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 22.4 kV/mm | 569 kV/in | ASTM D149 |
Multibase TPSiV™ 1180-50D Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Dielectric Strength | 22.4 kV/mm @Frequency 100 Hz |
569 kV/in @Frequency 100 Hz |
ASTM D149 |
Multibase TPSiV™ 1180-50D Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Dielectric Strength | 22.4 kV/mm | 570 kV/in | Short Term; ASTM D149 |
Quadrant EPP Semitron® MPR-1000 (ASTM Product Data Sheet) |
|||
Dielectric Strength | 22.4 kV/mm | 570 kV/in | |
Saint-Gobain CHR® G551 Glass Cloth Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Dielectric Strength | 22.4 kV/mm @Thickness 1.60 mm |
569 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL GTX GTX951W PPE+PA66 (Asia Pacific) A new high flow GTX designed for under-the-hood applications such as power distribution boxes, relay boxes and junction boxes. Developmental name: EXNX0151. |
|||
Dielectric Strength | 22.4 kV/mm | 569 kV/in | |
Covestro Desmopan® 460 Thermoplastic Polyurethane Desmopan 460 is a TPU on the basis of a special ester.Applications: Bearing shells, gear wheels, seals, cable connectors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience w.. |
|||
Dielectric Strength | 22.4 kV/mm | 570 kV/in | ASTM D149 |
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat.. |
|||
Dielectric Strength | 22.4 kV/mm | 570 kV/in | ASTM D149 |
Arlon HSLW301R##-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate.. |
|||
Dielectric Strength | 22.4 kV/mm | 570 kV/in | ASTM D149 |
Arlon HSLW401R##-P0 0.040" (1.02 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: High Strength, 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicate.. |
|||
Dielectric Strength | 22.4 kV/mm | 570 kV/in | ASTM D149 |
Arlon LW3015B##-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.5 inch wide, 30 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll leng.. |
|||
Dielectric Strength | 22.4 kV/mm | 570 kV/in | ASTM D149 |
Arlon P3272-10Rxx-P4 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Rectangular, Unsupported) Description: High strength self-fusing silicone tapeDesign/Construction: Interleave: PolyethyleneRubber: Cured Self-Fusing Silicone Rubber Cross-Section: 1” wide RectangularAppearance: Red silicone.. |
|||
Dielectric Strength | 22.4 kV/mm | 570 kV/in | ASTM D149 |
Arlon T4020-R002 0.020" Cured, Fusible Silicone Rubber with Fiberglass Substrate 0.5 inch wide, 20 mil thick, red, rectangular cross-section, fusible silicone tape.Design/Construction:Side 1: Cured Fusible Silicone RubberSubstrate: 15% Sinusoidal FiberglassSide 2: Cured Fusibl.. |
|||
Dielectric Strength | 22.4 kV/mm @Thickness 0.991 mm |
570 kV/in @Thickness 0.0390 in |
|
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Dielectric Strength | 22.4 kV/mm | 569 kV/in | Short Time; ASTM D149 |
Ascend Performance Materials VYDYNE® 21SP Nylon, General Purpose 1.4% Deformation under 14 MPa (2000 psi) load.Typical property data. VYDYNE is a registered trademark of Solutia Inc. |