Polymer Property : Dielectric Strength = 21.6 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 21.6 kV/mm

@Thickness 3.20 mm
549 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics NORYL HN731A PPE+PS
PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine..
Dielectric Strength 21.6 kV/mm

@Thickness 3.20 mm
549 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
Dielectric Strength 21.6 kV/mm

@Thickness 3.20 mm
549 kV/in

@Thickness 0.126 in
in oil; ASTM D 149
SABIC Innovative Plastics Noryl 731H PPE+PS
High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 21.6 kV/mm

@Thickness 3.20 mm
549 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics NORYL GFN3 PPE+PS
PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui..
Dielectric Strength 21.6 - 23.4 kV/mm
549 - 594 kV/in
UV Postcure; ASTM D149-97A
DSM Somos® NeXt LV Grey
The second member of the Somos® NeXt family, Somos® NeXt LV Grey delivers the durability and functionality, with a finer resolution of details and faster part processing. This third-generation, hi..