Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.50 kV/mm | 520.7 kV/in | |
Parker Chomerics CHO-SHIELD® 4968 Silicone Coating Silicone Coating. This is a two-component silicone polymer system used to protect electronic components and assemblies against moisture, abrasion, dust, and chemicals. It is particularly intended to.. |