Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 190 kV/mm @Temperature 23.0 °C |
4830 kV/in @Temperature 73.4 °F |
1/4 inch electrode; ASTM D149 |
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI.. |
|||
Dielectric Strength | 190 kV/mm | 4830 kV/in | MD, 6.25mm (0.25in) electrode; ASTM D149 |
Victrex® APTIV® 1300-050G Polyetheretherketone (PEEK) Polymer Film DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance .. |
|||
Dielectric Strength | 190 kV/mm | 4830 kV/in | TD, 6.25mm (0.25in) electrode; ASTM D149 |
Victrex® APTIV® 1300-050G Polyetheretherketone (PEEK) Polymer Film DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance .. |
|||
Dielectric Strength | 190 kV/mm @Temperature 23.0 °C |
4830 kV/in @Temperature 73.4 °F |
1/4 inch electrode; ASTM D149 |
Victrex® APTIV® 2000-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous APTIV PEEK 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV PEEK .. |
|||
Dielectric Strength | 190 kV/mm @Thickness 0.0250 mm |
4830 kV/in @Thickness 0.000984 in |
ASTM D149 |
Solvay Specialty Polymers Ajedium™ Films -- Radel® R-5100 NT15 Polyphenylsulfone (PPSU) Radel® polyphenylsulfone is an amorphous thermoplastic material that offers exceptional hydrolytic stability, and toughness superior to other commercially available, high-temperature films. PPSU .. |
|||
Dielectric Strength | 190 kV/mm | 4830 kV/in | MD, 6.25mm (0.25in) electrode; ASTM D149 |
Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance .. |
|||
Dielectric Strength | 190 kV/mm | 4830 kV/in | TD, 6.25mm (0.25in) electrode; ASTM D149 |
Victrex® APTIV® 1300-100G Polyetheretherketone (PEEK) Polymer Film DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance .. |