Electrical Properties Metric English Comments
Dielectric Strength 19.1 kV/mm
485 kV/in
ASTM D149
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide  (discontinued **)
Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol..
Dielectric Strength 19.1 kV/mm

@Thickness 3.20 mm
485 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® HR426 PBT
AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability.
Dielectric Strength 19.1 kV/mm

@Thickness 3.20 mm
485 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® HR426 PBT (Asia Pacific)
AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability.
Dielectric Strength 19.1 kV/mm
485 kV/in
Dow Corning 3-4133 DIELECTRIC GEL KIT
Two-part, clear, heat cure, and firm.Information provided by Dow Corning
Dielectric Strength >= 19.1 kV/mm
>= 486 kV/in
ASTM D149
Arlon 22122R079 0.079" Cured Silicone Rubber and FEP Film Laminate
Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: 0.005" FEP FilmThis data represents typical values for the production material and should not be used as ..
Dielectric Strength 19.1 kV/mm
485 kV/in
ASTM D149
Arlon 55106R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silic..
Dielectric Strength 19.1 kV/mm
485 kV/in
ASTM D149
Arlon 55146R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sili..
Dielectric Strength 19.1 kV/mm
486 kV/in
Short Time
Bulk Molding Compounds BMC 1410 Electrical Grade
BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally..
Dielectric Strength 19.1 kV/mm
486 kV/in
ASTM D149
Arlon R37732R079 0.079" (2.01 mm) Cured Silicone Rubber with FEP Film Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: FEP FilmAppearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical value..
Dielectric Strength 19.1 kV/mm
485 kV/in
ASTM D149
Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic..
Dielectric Strength 19.1 kV/mm
486 kV/in
ASTM D149
Arlon R37732W079 0.079" (2.01 mm) Cured Silicone Rubber with Treated FEP Film Substrate
Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Treated FEP FilmThis data represents typical values for the production material. The data should not be used to w..