Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.9 kV/mm | 480 kV/in | |
Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite MM 800 (formerly MM 1600) is a compression molded glass mica composite that is the perfect alternative to high performance plastics where high temperature, good dielectric strength and good arc resi.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Short Term; ASTM D149 |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Short Term; ASTM D149 |
Quadrant EPP Ketron® 1000 LSG PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Datasheet) |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | ASTM D149 |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Cured |
Resin Technology Group MX-2212 High Impact, Multi-Functional, UV Curing Adhesive This multi-functional product is a rapid setting structural adhesive. UV-MX 2212 provides high impact, resilient bonds to many similar and dissimilar substrates. Multi-functional cure bonds are form.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | |
ACC QSil 430 QSI Quantum Silicones Silicone Potting Material
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: 100% solid, quick curing, flame retardant, great adhesion to a variety of substrates. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | ASTM D149 |
Ravago Manufacturing Americas Hylon® N1040ML Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Dielectric Strength | 18.9 - 40.0 kV/mm | 480 - 1020 kV/in | Average value: 25.7 kV/mm Grade Count:5 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | |
Lord Adhesives Thermosetâ„¢ LS 213-9 Unfilled Epoxy Encapsulant Lord LS 213-9 is a one component epoxy coating and impregnating compound featuring low viscosity, good moisture resistance and excellent dielectric properties. Typical applications include transform.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Elastoblend® PA6/6 GF33 IM L NAT001 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedAppearance.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® ABS GF10 FR 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, I.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 GF13 FR BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® ABS GF10 A1 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF30 RM-1 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: Lubricated and Low Moisture AbsorptionInformation provided .. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PBT GF20 BK007 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 6225111Information provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | |
Saint-Gobain CHR® G565 Glass Cloth Backing Silicone Adhesive Pressure Sensitive Tape Description: Glass cloth offers excellent abrasion resistance and mechanical properties, as well as high tensile strength and extreme temperature resistance. Service temperatures range from -100°.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6/6 ML2 Nylon 66 Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES Luriblend® PA6/6 TL20 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Low Friction and Good Wear ResistanceUL File Number: E157318TPCI# 9740101Information provided by TP Compos.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PBT GF15 BK001 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: BlackTPCI# 6100111Information provided by TP Composit.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | ASTM D149-93 |
Saint-Gobain Versilicâ„¢ SPX-50 High Strength Silicone Tubing Formulation Description: Versilicâ„¢ SPX-50: Peroxide-cured Versilicâ„¢ High-Strength Silicone Tubing is designed for use in applications where flexibility, resiliency and durability are required. Its s.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | ASTM D149 |
Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) Polifil® GFABS series compounds combine the most desirable properties of both components - allowing for enhanced processability and toughness together with the stiffness of glass.Applications: Fire.. |
|||
Dielectric Strength | 18.9 kV/mm | 480 kV/in | ASTM D149 |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |