Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). UL94 V0, V2 and 5VA listing. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 1100F PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 1100R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 1110F PEI (Europe-Africa-Middle East) Enhanced flow PolyetherimiEnhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no long.. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 1110R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 1110V PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem MD130A PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, ISO 10993 compliant in recognized colors.This data was supplied by SABIC-IP for the Europe-.. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. |
|||
Dielectric Strength | 17.2 kV/mm @Thickness 3.20 mm |
437 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 17.2 kV/mm | 437 kV/in | |
Covestro Desmopan® 786 Thermoplastic Polyurethane Desmopan 786 is a TPU on the basis of a special carbonate with very good microbe-resistance.Applications: Tabular films, films, profiles.Information provided by Bayer.As of 1 September 2015, Bayer M.. |
|||
Dielectric Strength | 17.2 kV/mm | 438 kV/in | Short Time |
Bulk Molding Compounds BMC 1403 Electrical Grade BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo.. |
|||
Dielectric Strength | 17.2 kV/mm | 436 kV/in | Short Time |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Dielectric Strength | 17.2 - 20.3 kV/mm | 437 - 516 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories 95 Alumina Ceramic Tubes & Rods LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulat.. |
|||
Dielectric Strength | 17.2 kV/mm | 437 kV/in | Short Time; ASTM D149 |
Plenco 51015 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 51015 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL listed.Information supplied by.. |