Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 157 kV/mm | 4000 kV/in | ASTM D-149 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.001" thick) Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet.. |
|||
Dielectric Strength | 157 kV/mm | 4000 kV/in | ASTM D-149 |
Saint-Gobain Norton® Fluorglas® Chemfilm® R191 Skived Sintered PTFE Tape (0.002" thick) Description: Skived Sintered PTFE Films are used as barrier and insulation tapes for wire and cable, as well as the primary wall material for convoluted hose, Description: Skived sintered films meet.. |
|||
Dielectric Strength | 157 kV/mm | 4000 kV/in | ASTM D-149 |
Saint-Gobain Norton® PVDF Fluoropolymer Film Features/Benefits:Excellent weatherabilityHigh dielectric strengthExcellent chemical and abrasion resistanceThermoformableProduct available in widths up to 60"Product available with thicknesses from.. |
|||
Dielectric Strength | 157 kV/mm | 4000 kV/in | ASTM D149-97a |
Topas Advanced Polymers TOPAS® Elastomer E-140 Developmental Cyclic Olefin Copolymer (COC) TOPAS® Elastomer E-140, unlike most TOPAS grades, is a semicrystalline cyclic olefin material with flexibility. It is a fairly stiff elastomer which can be extruded and injection molded, and can be.. |
|||
Dielectric Strength | 157 kV/mm | 3990 kV/in | |
Von Roll Isola IMI Varnish 708 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 76°C. Usag.. |
|||
Dielectric Strength | 157 kV/mm | 4000 kV/in | 0.25 inch electrodes in dry air @25°C; ASTM D149-81 |
DuPont Teijin Films Melinex® S Polyester Film, 300 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Dielectric Strength | 157 kV/mm | 4000 kV/in | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Melinex® SWC Polyester Film, 300 Gauge A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi.. |