Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
Rogers Corporation Ultralam® 3908 Liquid Crystalline Polymer Circuit Material
ULTRALAM® 3908 bondply is used as a bonding medium between copper and the dielectric material. This product was developed specifically for multi-layer substrate constructions. This adhesiveless f..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D-149
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.002" thick)
T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele..
Dielectric Strength 118 kV/mm
3000 kV/in
Saint-Gobain CHR® K290ESD Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D-149
Saint-Gobain Norton® T-100 Virgin Skived PTFE Film (0.001" thick)
T-100/T-200 Features/Benefits: Outstanding heat and chemical resistance; High dielectric strength; Anti-stick properties; Can be chemically etched for bondability; Applications include laminate rele..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
Cytec CC-1191 (Conap) Acrylic Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
Cytec CE-1170 (Conap) Acrylic Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
Cytec CE-1171 (Conap) Acrylic Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
Cytec Conathane® CC-1155 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
Cytec Conathane® CC-1155-35 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
Cytec Conathane® CC-1195 (Conap) Polyurethane Two-component Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D151-81
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film
Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D151-81
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D151-81
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film
UV Screening, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistan..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D151-81
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film
Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST504 Polyester Film, 500 Gauge
Melinex® ST504 is a crystal clear, high gloss, heat stabilized polyester film. It can be overprinted with a wide range of solvent-based graphic inks and varnishes, silver conductive and dielectric ..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST504 Polyester Film, 700 Gauge
Melinex® ST504 is a crystal clear, high gloss, heat stabilized polyester film. It can be overprinted with a wide range of solvent-based graphic inks and varnishes, silver conductive and dielectric ..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST505 Polyester Film, 500 Gauge
Melinex® ST505 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST505 Polyester Film, 700 Gauge
Melinex® ST505 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST506 Polyester Film, 500 Gauge
Melinex® ST506 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic..
Dielectric Strength 118 kV/mm
3000 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Melinex® SWC Polyester Film, 500 Gauge
A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi..
Dielectric Strength 118 kV/mm
3000 kV/in
ASTM D149
DuPont Teijin Films Melinex® ST506 Polyester Film, 700 Gauge
Melinex® ST506 is a crystal clear, high gloss, heat stabilized polyester film. It is pretreated on both sides for improved adhesion. It can be overprinted with a wide range of solvent-based graphic..
Dielectric Strength >= 118 kV/mm
>= 3000 kV/in
Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u..
Copyright © lookpolymers.com All Rights Reserved