Polymer Property : Dielectric Strength = 1170 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 46.0 kV/mm

@Thickness 1.00 mm
1170 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics NORYL NH5110E PPE+PS (Europe-Africa-Middle East)
NORYL NH5110E is a flame retardant, non halogenated, impact modified extrusion grade. Developed for low beard-growth, with a Vicat B/120 of 138 Deg C, according to ISO 306 and a UL-94 rating of V1@ ..
Dielectric Strength 46.0 kV/mm
1170 kV/in
IEC 60243-1 3
BASF Ultrason S 2010 G4 20% Glass Filled PSU
Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Dielectric Strength 46.0 kV/mm
1170 kV/in
Breakdown
Advanced Ceramics ACL 2087 Lithium Alumino-Silicate
A high strength glass-ceramic suitable for sealing to 17% chrome-iron or Nilo 48Information provided by Advanced Ceramics Limited (ACL)
Dielectric Strength 46.0 kV/mm
1170 kV/in
DIN 53481/VDE 0303
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...
Dielectric Strength 46.0 kV/mm
1170 kV/in
IEC 243
LG Chemical HF-380 ABS, High Flow, High Impact
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products, Toys, Miscellaneous Goods)CAS No. 9003-56-9Information Provided by LG Chem