Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 81.0 - 150 mm/min @Thickness 3.05 mm |
3.19 - 5.91 in/min @Thickness 0.120 in |
UL PLC 3 (81-150 mm/min) |
Resinoid 2016 Phenolic Molding, Fabric Reinforced Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance |