Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 50.0 mm/min | 0.394 - 1.97 in/min | Average value: 32.7 mm/min Grade Count:4 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical HIPS MI750L PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMAX HR5107 PBT+ABS+GF10%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF10%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5, 25038-59-9 and 9003-54-7Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General PurposeApplication: HMID, SLMP B, HolderCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupox® GP2400G PBT+GF40% Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1301EP30 Polycarbonate Resin Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1303EP-22 Polycarbonate Resin Description: LUPOY PC 1303EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1303-07 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1303-10 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min | |
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |