Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Cycolac® X15 ABS Automotive. Very high heat resistance with high impact. UL94 HB rated. High gloss.This data was supplied by SABIC-IP for the Americas region. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 103 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 103 PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 123R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 203R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 223R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® 223S PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Lexan® LS1 PC (Asia Pacific) Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Lexan® 151 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=0.750 mm |
7.0 - 15 sec @Thickness >=0.0295 in |
|
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2310EPR PEI (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | PLC code 4; UL 746A |
SABIC Innovative Plastics LNP Thermocomp RF00ASXP PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RF00ASXP is a compound based on PA 66 resin containing Glass Fiber. Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics NORYL GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | UL 746A |
SABIC Innovative Plastics Valox® V3504 PBT (Asia Pacific) VALOX EXVX0197 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
DuPont Teijin Films Mylar® EL21 Polyester Film, 1400 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Hot Wire Ignition, HWI | 7.0 - 15 sec | 7.0 - 15 sec | |
DuPont Teijin Films Mylar® EL21 Polyester Film, 900 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |