Electrical Properties Metric English Comments
Dielectric Breakdown 9000 V
9000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b..
Dielectric Breakdown 9000 V
9000 V
Saint-Gobain CHR® 2285-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Dielectric Breakdown 9000 V
9000 V
Saint-Gobain CHR® 2355-2 FEP Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: FEP film is used for applications requiring optical clarity, quick release, and abrasion resistance. FEP film applications include high temperature coil and capacitor wrapping, composit..
Dielectric Breakdown 9000 V
9000 V
Saint-Gobain CHR® C Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: FEP film is used for applications requiring optical clarity, quick release, and abrasion resistance. FEP film applications include high temperature coil and capacitor wrapping, composit..
Dielectric Breakdown 9000 V
9000 V
Saint-Gobain CHR® 2254-2 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Dielectric Breakdown 9000 V
9000 V
Saint-Gobain CHR® 2255-2 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Dielectric Breakdown >= 9000 V
>= 9000 V
IEC 626
Dr. D. Mueller Flexiso® DMD FI 14010 00210 Polyester Electrical Insulation
Structure: Flexiso® DMD, FI 14010 00210 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with ..
Dielectric Breakdown 9000 V
9000 V
High Humidity; ASTM D1000
3M Scotch® Super 88 Vinyl Electrical Tape
Scotch® Vinyl Electrical Tape Super 88 is a premium grade, 8.5 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape is..
Copyright © lookpolymers.com All Rights Reserved