Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 8400 V | 8400 V | Dielectric Strength |
Dielectric Polymers NT-490 Polyimide Label Stock
(discontinued **) High temperature acrylic adhesive with thermal transfer imprintable polyimide film backing.Features: Meets ANSI standards for print contract signals and minimum reflectance ratios for bar code print.. |