Electrical Properties Metric English Comments
Dielectric Breakdown 6500 V
6500 V
Dielectric Strength
Dielectric Polymers NT-8512-2 Powder Coating Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista..
Dielectric Breakdown 6500 V
6500 V
Dielectric Strength
Dielectric Polymers NT-9512 Powder Coating Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityNo film shrinkage after exposure to elevated temperaturesAbrasion resista..
Dielectric Breakdown 6500 V
6500 V
Dielectric Strength
Dielectric Polymers NT-9512-2DL Selective Masking Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: High temperature resistantDie cut disks/shapes remove easily from linerClean tape removalApplications: For selective masking appli..
Dielectric Breakdown 6500 V
6500 V
Saint-Gobain CHR® 2345-1 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
Dielectric Breakdown 6500 V
6500 V
Saint-Gobain CHR® SG03-06(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Dielectric Breakdown 6500 V
6500 V
Saint-Gobain CHR® SG05-06(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Dielectric Breakdown 6500 V
6500 V
Saint-Gobain CHR® SG06-06(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..