Polymer Property : Dielectric Breakdown = 6000 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown 6000 V
6000 V
Withstand Voltage [V/min]; AC 60 Hz
Fujipoly Industries Sarcon® 20GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Breakdown 6000 V
6000 V
Withstand Voltage [V/min]; AC 60 HZ
Fujipoly Industries Sarcon® 30H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Breakdown 6000 V
6000 V
Withstand Voltage [V/min]; AC 60 HZ
Fujipoly Industries Sarcon® 30U Thin-Film UR
Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
Dielectric Breakdown >= 6000 V
>= 6000 V
Withstand Voltage AC V
Fujipoly Industries DELTA-5TV-20-1 silicone rubber fusible tape
Information provided by Fujipoly Industries
Dielectric Breakdown 6000 V
6000 V
Saint-Gobain CHR® M851 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Breakdown 6000 V
6000 V
100 V/sec
DuPont Teijin Films Mylar® C Polyester Film, 92 Gauge
Mylar® Type C films are available in a wide range of generally thinner gauges (typically 10 through 92) that offer excellent electrical properties, combined with superior strength and dimensional s..