Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 54000 V | 54000 V | Parallel, Step-By-Step in Oil; ASTM D149 |
Haysite H722 Polyester, Glass Reinforced H722 is an all-purpose GPO-1 fiberglass mat reinforced thermoset polyester molded sheet. Available in thicknesses ranging from .031" - 2.00". Standard color - Natural. Meets Gov't Specs - LP-509, .. |