Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 1500 - 8400 V | 1500 - 8400 V | Average value: 2990 V Grade Count:7 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dielectric Breakdown | 1500 V | 1500 V | Average value: 1500 V Grade Count:7 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Breakdown | 1500 V | 1500 V | Average value: 1500 V Grade Count:5 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1A20 Urethane Conformal Coating Humiseal 1A20 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1A20LSE Urethane Conformal Coating Humiseal 1A20LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval pendingPasses ther.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1A27 Urethane Conformal Coating Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1A27LSE Urethane Conformal Coating Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C).. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1A33 Urethane Conformal Coating Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1A33LSE Urethane Conformal Coating Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1B12 Acrylic Conformal Coating Humiseal 1B12 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityPasses thermal shock test (MIL-I-46058C)Flammabili.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1B31 Acrylic Conformal Coating Humiseal 1B31 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C ApprovedPasses thermal shock test (MI.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1B31LSE Acrylic Conformal Coating Humiseal 1B31LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C Approval PendingPasses thermal sho.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1B73 Acrylic Conformal Coating Humiseal 1B73 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL ApprovedMIL-I-46058C ApprovedPasses thermal sho.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1B73LSE Acrylic Conformal Coating Humiseal 1B73LSE Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL Approval PendingMIL-I-46058C Approval Pendin.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1C49 Silicone Conformal Coating Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1C51 Silicone Conformal Coating Humiseal 1C51 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1C55 Silicone Conformal Coating Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1C61 UV Cure Conformal Coating Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t.. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 1C65 Silicone Conformal Coating Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Dielectric Breakdown | >= 1500 V | >= 1500 V | Dielectric Withstand; MIL-I-46058C |
Humiseal 2A64 Urethane Conformal Coating Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F.. |