Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 11000 V | 11000 V | Withstand Voltage [V/min]; AC 60 Hz |
Fujipoly Industries Sarcon® 85Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Breakdown | 11000 V | 11000 V | Withstand Voltage [V/min]; AC 60 Hz |
Fujipoly Industries Sarcon® 85U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Breakdown | 11000 V | 11000 V | Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-Hn Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Breakdown | 11000 V | 11000 V | Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Dielectric Breakdown | 11000 V | 11000 V | Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® XR-e Gap Filler Pad Sarcon XR-e and XR-j are highly conformable/thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of compon.. |
|||
Dielectric Breakdown | 11000 V | 11000 V | Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® XR-j Gap Filler Pad Sarcon XR-e and XR-j are highly conformable/thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of compon.. |
|||
Dielectric Breakdown | 11000 V | 11000 V | |
Saint-Gobain CHR® 2275-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Dielectric Breakdown | 11000 V | 11000 V | |
Saint-Gobain CHR® 2255-3 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |