Electrical Properties Metric English Comments
Dielectric Breakdown >= 1000 V

@Temperature 90.0 °C
>= 1000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Hippe PF CC 203 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts. Better mechanical properties and poorer electrical properties than type PF CC 204.Information ..
Dielectric Breakdown >= 1000 V

@Temperature 90.0 °C
>= 1000 V

@Temperature 194 °F
In oil, parallel to laminations; IEC 1212-2 6.2
Hippe PF CC 201 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical applications (coarse weave: >130 g/m2, =30 threads/cm). Better mechanical properties and poorer electrical properties than type PF CC 202.Information provided by Hippe.
Dielectric Breakdown >= 1000 V
>= 1000 V
Standard condition; ASTM D1000
3M Temflex™ 1700 Vinyl Electrical Tape
Scotch® Vinyl Electrical Tape 1700 is a good quality, economical general purpose vinyl insulating tape. It has excellent resistance to: abrasion, moisture, alkalies, acid, copper corrosion and vary..
Dielectric Breakdown >= 1000 V
>= 1000 V
Standard condition; ASTM D1000
3M Temflex™ 1776 Vinyl Electrical Tape
3M™ Temflex™ Vinyl Electrical Tape 1776 is a good quality, economical, general-purpose vinyl insulating tape, manufactured in the USA. It has excellent resistance to abrasion, moisture, alkalies, ..