Polymer Property : Insulation Resistance = 5.00e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance 5.00e+14 ohm
5.00e+14 ohm
Average value: 5.00e+14 ohm Grade Count:5
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
Insulation Resistance 5.00e+14 ohm
5.00e+14 ohm
Insulation Resistance; MIL-I-46058C
Humiseal 1C49 Silicone Conformal Coating
Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605..
Insulation Resistance 5.00e+14 ohm
5.00e+14 ohm
Insulation Resistance; MIL-I-46058C
Humiseal 1C51 Silicone Conformal Coating
Humiseal 1C51 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605..
Insulation Resistance 5.00e+14 ohm
5.00e+14 ohm
Insulation Resistance; MIL-I-46058C
Humiseal 1C55 Silicone Conformal Coating
Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock ..
Insulation Resistance 5.00e+14 ohm
5.00e+14 ohm
Insulation Resistance; MIL-I-46058C
Humiseal 1C61 UV Cure Conformal Coating
Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t..
Insulation Resistance 5.00e+14 ohm
5.00e+14 ohm
Insulation Resistance; MIL-I-46058C
Humiseal 1C63 Silicone Conformal Coating
Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock ..
Insulation Resistance 5.00e+14 ohm
5.00e+14 ohm
Insulation Resistance; MIL-I-46058C
Humiseal 1C65 Silicone Conformal Coating
Humiseal 1C65 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock ..