Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 2.70e+14 ohm @Temperature 60.0 °C |
2.70e+14 ohm @Temperature 140 °F |
50% RH |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Insulation Resistance | 2.70e+14 ohm @Temperature 60.0 °C |
2.70e+14 ohm @Temperature 140 °F |
50% RH |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Insulation Resistance | 2.70e+14 ohm @Temperature 60.0 °C |
2.70e+14 ohm @Temperature 140 °F |
50% RH |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Crossply CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |