Polymer Property : Insulation Resistance = 1.00e+15 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Before moisture resistance, test voltage = 100 VDC, MIL-I-46058C
3M 941 Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Insulation Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Before moisture resistance, test voltage = 100 VDC, MIL-I-46058C
3M 9461P Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Insulation Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Before moisture resistance, test voltage = 100 VDC, MIL-I-46058C
3M 9461PC Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Insulation Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Before moisture resistance, test voltage = 100 VDC, MIL-I-46058C
3M 965 Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Insulation Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Before moisture resistance, test voltage = 100 VDC, MIL-I-46058C
3M 966 Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Insulation Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
Before moisture resistance, test voltage = 100 VDC, MIL-I-46058C
3M 9462P Adhesive Transfer Tapes with Adhesive 100
These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va..
Insulation Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Vyncolit INSUL-PLATE™ X-28057-2HT Hole-Fill Powder For Printed Circuit Boards
Vyncolit INSUL-PLATE™ Hole-Fill material delivers true reliability and superior performance. This material, in powder form, is specifically suited for Hole-Fill use in glass epoxy, multi-layer and ..