Polymer Property : Insulation Resistance = 1.00e+12 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance 100 - 1.00e+12 ohm
100 - 1.00e+12 ohm
Average value: 2.23e+10 ohm Grade Count:70
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Insulation Resistance 1.00e+9 - 1.00e+12 ohm
1.00e+9 - 1.00e+12 ohm
Average value: 9.29e+11 ohm Grade Count:14
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Insulation Resistance 1.00e+11 - 1.00e+12 ohm
1.00e+11 - 1.00e+12 ohm
Average value: 4.60e+11 ohm Grade Count:5
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Insulation Resistance 100 - 1.00e+12 ohm
100 - 1.00e+12 ohm
Average value: 7.14e+10 ohm Grade Count:28
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Insulation Resistance 1.00e+9 - 1.00e+12 ohm
1.00e+9 - 1.00e+12 ohm
Average value: 2.78e+11 ohm Grade Count:4
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Insulation Resistance 1.00e+8 - 1.00e+12 ohm
1.00e+8 - 1.00e+12 ohm
Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
Insulation Resistance 1.00e+9 - 1.00e+12 ohm
1.00e+9 - 1.00e+12 ohm
Average value: 8.42e+11 ohm Grade Count:12
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Insulation Resistance 100000 - 1.00e+12 ohm
100000 - 1.00e+12 ohm
Average value: 6.88e+11 ohm Grade Count:16
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Insulation Resistance 1000 - 1.00e+12 ohm
1000 - 1.00e+12 ohm
Average value: 7.08e+11 ohm Grade Count:24
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Insulation Resistance 1.00e+11 - 1.00e+12 ohm

@Temperature 90.0 - 90.0 °C
1.00e+11 - 1.00e+12 ohm

@Temperature 194 - 194 °F
Average value: 5.15e+11 ohm Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..