Electrical Properties Metric English Comments
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
Method B (Step-by-Step); ASTM D149
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat..
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East)
VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries.
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot..
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East)
VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto..
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East)
VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics.
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East)
VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics.
Dielectric Strength 29.0 kV/mm

@Thickness 2.00 mm
737 kV/in

@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 29.0 kV/mm

@Thickness 2.00 mm
737 kV/in

@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 29.0 kV/mm

@Thickness 2.00 mm,
Temperature 23.0 °C
737 kV/in

@Thickness 0.0787 in,
Temperature 73.4 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..
Dielectric Strength 29.0 kV/mm

@Thickness 0.800 mm
737 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East)
VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes.