Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 700 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 27.6 kV/mm

@Thickness 1.59 mm
700 kV/in

@Thickness 0.0625 in
in oil; ASTM D149
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant
Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Dielectric Strength 27.6 kV/mm

@Thickness 1.57 mm
700 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP159 Synthetic Fabric  (discontinued **)
Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit..
Dielectric Strength 27.6 kV/mm

@Thickness 1.57 mm
700 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
Industrial Laminates/Norplex NP130HF Glass Fabric
Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens..
Dielectric Strength 27.6 kV/mm

@Thickness 1.57 mm
700 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP630 Paper Base Laminate
Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500"
Copyright © lookpolymers.com All Rights Reserved