Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 26.4 kV/mm @Thickness 1.60 mm |
671 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 26.4 kV/mm @Thickness 1.60 mm |
671 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 26.4 kV/mm @Thickness 1.60 mm |
671 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 26.4 kV/mm @Thickness 1.60 mm |
671 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Valox® 414 PBT (Asia Pacific) 40% GR, increased strength/stiffness vs unreinforced. Non-flame retardant. For appliance handles, spotlights, electric motors, pump housings etc.This data was supplied by SABIC-IP for the Asia Pacif.. |