Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 46.0 kV/mm @Thickness 0.800 mm |
1170 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Dielectric Strength | 46.0 kV/mm @Thickness 0.800 mm |
1170 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Dielectric Strength | 46.0 kV/mm @Thickness 0.800 mm |
1170 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Dielectric Strength | 46.0 kV/mm @Thickness 0.800 mm |
1170 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Dielectric Strength | 46.0 kV/mm @Thickness 0.800 mm |
1170 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific) CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Dielectric Strength | 46.0 kV/mm @Thickness 0.800 mm |
1170 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
Dielectric Strength | 46.0 kV/mm @Thickness 0.500 mm |
1170 kV/in @Thickness 0.0197 in |
Transformer Oil; IEC 60243-1 |
SYNTHOS Forsan® 393 Acrylonitrile Butadiene Styrene (ABS) High heat resistance, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Ka.. |