Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 45.0 kV/mm @Thickness 0.500 mm |
1140 kV/in @Thickness 0.0197 in |
Transformer Oil; IEC 60243-1 |
SYNTHOS Forsan® 483 Acrylonitrile Butadiene Styrene (ABS) High heat resistant, high gloss.Applications: Electrotechnics, lighting equipment, automotiveHousehold appliances, electric switches, lamps, car interior parts, etc.Synthos was formerly known as Kau.. |