Polymer Property : Dielectric Strength = 38.0 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 38.0 kV/mm

@Thickness 0.800 mm
965 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Dielectric Strength 38.0 kV/mm

@Thickness 0.800 mm
965 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Asia Pacific)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Dielectric Strength 38.0 kV/mm

@Thickness 0.800 mm
965 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East)
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Dielectric Strength 38.0 kV/mm

@Thickness 0.800 mm
965 kV/in

@Thickness 0.0315 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
Dielectric Strength 38.0 kV/mm

@Thickness 0.800 mm
965 kV/in

@Thickness 0.0315 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend
Dielectric Strength 38.0 kV/mm

@Thickness 1.00 mm,
Temperature 23.0 °C
965 kV/in

@Thickness 0.0394 in,
Temperature 73.4 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..
Dielectric Strength 38.0 kV/mm

@Thickness 1.00 mm,
Temperature 90.0 °C
965 kV/in

@Thickness 0.0394 in,
Temperature 194 °F
IEC 60243-1
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..