Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 36.0 kV/mm @Thickness 0.800 mm |
914 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 0.800 mm |
914 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
914 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 1.00 mm, Temperature 90.0 °C |
914 kV/in @Thickness 0.0394 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 0.800 mm |
914 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Dielectric Strength | 36.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
914 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |