Polymer Property : Dielectric Strength = 328 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 12.9 kV/mm

@Frequency 60.0 Hz
328 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation proper-ties that meets the requir..
Dielectric Strength 12.9 kV/mm

@Frequency 60.0 Hz
328 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
Sumitomo Bakelite North America Epiall® 1960B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 1960B-1 is a mineral and short fiberglass filled epoxy compound, formulated for the encapsulation of passive electronic devices.Information provided by Sumitomo Bak North America, Inc.
Dielectric Strength 12.9 kV/mm

@Frequency 60.0 Hz
328 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information ..