Electrical Properties Metric English Comments
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000F PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D 149
SABIC Innovative Plastics Ultem 1000FV PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D 149
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D 149
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D 149
SABIC Innovative Plastics Ultem 1000M PEI
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D 149
SABIC Innovative Plastics Ultem 1000M PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000P PEI
Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000P PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000R PEI
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000R PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000RV PEI
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D 149
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be ..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1010F PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1010F PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer be ..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1010R PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D 149
SABIC Innovative Plastics Ultem 1010RF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion.
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM HU1000 PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI)..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM HU1010 PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000 PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20..
Dielectric Strength 32.7 kV/mm

@Thickness 1.60 mm
831 kV/in

@Thickness 0.0630 in
in air; ASTM D149
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer..