Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.6 kV/mm @Thickness 1.57 mm |
600 kV/in @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S.T. |
Industrial Laminates/Norplex NP630 Paper Base Laminate Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.57 mm |
600 kV/in @Thickness 0.0620 in |
D-48/50 |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.57 mm |
600 kV/in @Thickness 0.0620 in |
Cond A; ASTM D229 S.T. |
Industrial Laminates/Norplex NP634 Laminate Description: Warm punching, composite grade with woven glass covers for improved flexural, tensile and impact strength. Electrical properties comparable to NP611.Thickness Tested: 0.062", 0.125" and.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.60 mm |
599 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 457 PBT 6.5% GR PBT, UL94 V-0/5V. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.60 mm |
599 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific) 6.5% GR PBT, UL94 V-0/5V. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.20 mm |
599 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 508 PBT+PC 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.20 mm |
599 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 508R PBT+PC 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-FR. Reduced warpage characteristics. Applications same as VALOX 420R. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.20 mm |
599 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Valox® 735 PBT 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.20 mm |
599 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific) 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.20 mm |
599 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 735 PBT+PET 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.60 mm |
599 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.60 mm |
599 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 3.20 mm |
599 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 1.60 mm |
599 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.635 mm |
600 kV/in @Thickness 0.0250 in |
60 cycles AC avg. RMS; ASTM-D149 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.635 mm |
600 kV/in @Thickness 0.0250 in |
ASTM-D116 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 9667MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 7952MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Dielectric Strength | 23.6 kV/mm @Thickness 0.127 mm |
600 kV/in @Thickness 0.00500 in |
ASTM D149-92 |
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |