Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS (Europe-Africa-Middle East) PC+ABS, Industrial quality resin with good flow, good temperature resistance and moderate ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 310 PBT Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Unreinforced, general purpose. Typical viscosity 5000-7000. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310HP PBT PBT for compounding/fibers only. Not intended for injection molding. FDA compliant. Available in Natural color (1001) only. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 311 PBT Unreinforced, improved resistance to UV. Medium viscosity. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Valox® 312 PBT Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific) Unreinforced, For compounding only (not for injection molding), Medium viscosity. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 315 PBT Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 3.20 mm |
589 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 745 PBT 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 865 PBT+PET 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific) 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® DR51 PBT 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® DR51 PBT (Asia Pacific) 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in oil; ASTM D 149 |
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific) 15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia .. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 3.20 mm |
589 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 745 PBT (Asia Pacific) 30% mineral reinforced polyester improved toughness and low warpage. Typical applications are telephone ringer frames and card racks. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in air; ASTM D149 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in air; ASTM D149 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Dielectric Strength | 23.2 kV/mm @Thickness 1.60 mm |
589 kV/in @Thickness 0.0630 in |
in air; ASTM D149 |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |