Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm, Temperature 23.0 °C |
559 kV/in @Thickness 0.0630 in, Temperature 73.4 °F |
Short Time; ASTM D149 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.00 mm |
559 kV/in @Thickness 0.0394 in |
Conditioned; IEC 60243-1 |
Lanxess Durethan® BKV 15 H3.0 000000 Nylon 6 Copolymer, 15% Glass Fibers PA 6 Copolymer, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 457 PBT (Europe-Africa-Middle East) VALOX 457 is a 6.5% glass fibre reinforced flame retarded PBT injection moulding resin. Applications: electrical and appliances industries. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 3.20 mm |
559 kV/in @Thickness 0.126 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Valox® 701 PBT (Asia Pacific) 35% glass/mineral alloy, excellent electrical performance to dielectric breakdown. Developed for automotive distributor caps.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 3.20 mm |
559 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 3.20 mm |
559 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East) Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East) VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 1.60 mm |
559 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East) Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E.. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 0.800 mm |
559 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 3.20 mm |
559 kV/in @Thickness 0.126 in |
in air; ASTM D149 |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm |
559 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 1.9%); ASTM-D149 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 22.0 kV/mm @Temperature 23.0 °C |
559 kV/in @Temperature 73.4 °F |
50%RH; IEC 60243-1 |
DuPont Performance Polymers Zytel® ST801AW BK195 Nylon 66
(Unverified Data**) Zytel® ST801AW BK195 is a Super Tough, weatherable, easy flow and processing friendly, black polyamide 66 resin for injection molding. It offers the best resistance to outdoor exposure.Information.. |
|||
Dielectric Strength | 22.0 kV/mm @Temperature 100 °C |
559 kV/in @Temperature 212 °F |
IEC 60243/1 |
BASF Ultramid® A3EG10 High Speed Information provided by BASF |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm, Temperature 90.0 °C |
559 kV/in @Thickness 0.0787 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Dielectric Strength | 22.0 kV/mm @Thickness 2.00 mm, Temperature 90.0 °C |
559 kV/in @Thickness 0.0787 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |