Dielectric Strength 20.0 kV/mm

@Thickness 1.00 mm
508 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® 3414R PC (Europe-Africa-Middle East)
LEXAN 3414R is a high viscosity, 40% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance.
Dielectric Strength 20.0 kV/mm

@Thickness 1.57 mm
508 kV/in

@Thickness 0.0620 in
ASTM D149
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded  (d
AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, ..
Dielectric Strength 20.0 kV/mm

@Thickness 1.00 mm
508 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East)
LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
Dielectric Strength 20.0 kV/mm

@Thickness 1.00 mm
508 kV/in

@Thickness 0.0394 in
short time; IEC 60243-1
SABIC Innovative Plastics Lexan® ML3999 PC (Europe-Africa-Middle East)
LEXAN ML3999 is a medium viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
Dielectric Strength 20.0 kV/mm

@Thickness 1.60 mm
508 kV/in

@Thickness 0.0630 in
Method B (Step-by-Step); ASTM D149
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat..
Dielectric Strength 20.0 kV/mm

@Thickness 3.18 mm
508 kV/in

@Thickness 0.125 in
Method A (Short-Time); ASTM D149
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat..
Dielectric Strength 20.0 kV/mm

@Thickness 3.20 mm
508 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East)
VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications.
Dielectric Strength 20.0 kV/mm

@Thickness 3.20 mm
508 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East)
VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications.
Dielectric Strength 20.0 kV/mm

@Thickness 3.20 mm
508 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East)
VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin.
Dielectric Strength 20.0 kV/mm

@Thickness 3.20 mm
508 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 855 PBT
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
Dielectric Strength 20.0 kV/mm

@Thickness 3.20 mm
508 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Valox® 855 PBT (Asia Pacific)
15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts.
Dielectric Strength 20.0 kV/mm

@Thickness 3.20 mm
508 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Xenoy® 6370 PBT+PC
30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility.
Dielectric Strength 20.0 kV/mm

@Thickness 1.60 mm
508 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific)
XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r..
Dielectric Strength 20.0 kV/mm

@Thickness 1.60 mm
508 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East)
VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin.
Dielectric Strength 20.0 kV/mm

@Thickness 1.60 mm
508 kV/in

@Thickness 0.0630 in
in oil; IEC 60243-1
SABIC Innovative Plastics Valox® 4512 PBT+PC (Europe-Africa-Middle East)
10% GF FR PBT/PC Blend
Dielectric Strength 20.0 kV/mm

@Thickness 2.00 mm
508 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 2.3%); ASTM-D149
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 20.0 kV/mm

@Thickness 2.00 mm
508 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 2.5%); ASTM-D149
Toyobo GLAMIDE® T-521 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 20.0 kV/mm

@Thickness 2.00 mm
508 kV/in

@Thickness 0.0787 in
Absolute Drying; ASTM-D149
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 20.0 kV/mm

@Thickness 2.00 mm
508 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 1.75%); ASTM-D149
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 20.0 kV/mm

@Thickness 2.00 mm
508 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 0.8%); ASTM-D149
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 20.0 kV/mm

@Thickness 2.00 mm
508 kV/in

@Thickness 0.0787 in
Practical Use (Water Absorption 1.8%); ASTM-D149
Toyobo GLAMIDE® T-422VOR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Dielectric Strength 20.0 kV/mm

@Thickness 3.00 mm
508 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Elektro-Isola Etronax P EP Phenolic, Polyester Fabric Reinforcement, Light Yellow, Sheets
Description: This material is exceptionally strong and tough. Very low water absorption and the lowest swelling in water. High resistance to chemicals, including SF6 gas. Applications: Can be used i..
Dielectric Strength 20.0 kV/mm

@Thickness 3.00 mm
508 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets
Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation ..
Copyright © lookpolymers.com All Rights Reserved