Polymer Property : Dielectric Strength = 1220 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 48.0 kV/mm

@Thickness 0.500 mm
1220 kV/in

@Thickness 0.0197 in
Transformer Oil; IEC 60243-1
SYNTHOS Forsan® 573 Acrylonitrile Butadiene Styrene (ABS)
Increased heat resistant, glossy, good mechanical properties, suitable for electroplating.Applications: Electrotechnics, automotiveHousehold appliances, electric switches, car interior parts, profil..
Dielectric Strength 48.0 kV/mm

@Thickness 0.760 mm
1220 kV/in

@Thickness 0.0299 in
stepwise tension increase; ASTM D149-75
Arkema Group VOLTALEF® 300 HD PCTFE
VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group
Dielectric Strength 48.0 kV/mm

@Thickness 0.760 mm
1220 kV/in

@Thickness 0.0299 in
stepwise tension increase; ASTM D149-75
Arkema Group VOLTALEF® 302 PCTFE
VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group