Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.0 kV/mm @Temperature 121 °C, Time 10800 sec |
254 kV/in @Temperature 250 °F, Time 3.00 hour |
0.125 in. thickness; ASTM D149 |
Garlock 2900 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation .. |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.00 mm |
254 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.00 mm |
254 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola Etronit IV Phenolic, Paper Reinforcement, Yellow, Sheets Description: Grade for mechanical electrotechnical and high frequency purposes. Tropical grade, well suited for areas where high air humidity can be expected. Suitable as high-frequency insulation o.. |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.00 mm |
254 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.00 mm |
254 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica.. |
|||
Dielectric Strength | 10.0 kV/mm @Thickness 3.00 mm |
254 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60245-1; IEC/EN 60893-2 6.1.3.1 |
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope.. |