Polymer Property : Shielding Effectiveness = 65 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS003 ABS
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS003 PP
LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East)
LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS
LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Asia Pacific)
LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East)
LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS
LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta..
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Asia Pacific)
LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta..
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Europe-Africa-Middle East)
LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta..
Shielding Effectiveness 50 - 65 dB

@Thickness 3.00 mm
50 - 65 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex NS0039XP PC+ABS (Europe-Africa-Middle East)
LNP* FARADEX* NS0039XP is a compound based on PC/ABS resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Electrically Conductive, EMI/RFI Shielding, Flame retardant.Thi..