Electrical Properties Metric English Comments
Shielding Effectiveness 80 dB

@Frequency 1.00e+10 Hz
80 dB

@Frequency 1.00e+10 Hz
P-Field
P & P Technology Monel-BS3075 (NA13) Knitted Cored Shielding Mesh
Product has a diameter of 0.11mm.Information provided by P & P Technology
Shielding Effectiveness >= 80 dB

@Frequency 1.00e+10 Hz
>= 80 dB

@Frequency 1.00e+10 Hz
MIL-DTL-83528 Para.4.6.12
Parker Chomerics CHO-SEAL 1401 Conductive Elastomer
High performance for non-corrosive environments; soft(45 Shore A) for low closure force where gasket geometry cannot be exploited; low tear strength; no fluid resistance. Molded and ExtrudedRoHS Com..
Shielding Effectiveness >= 80 dB

@Frequency 1.00e+8 Hz
>= 80 dB

@Frequency 1.00e+8 Hz
E-Field; Method 3, CHO-TM-TP09
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer
Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast..
Shielding Effectiveness >= 80 dB

@Frequency 5.00e+8 Hz
>= 80 dB

@Frequency 5.00e+8 Hz
E-Field; Method 3, CHO-TM-TP09
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer
Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast..
Shielding Effectiveness >= 80 dB

@Frequency 2.00e+9 Hz
>= 80 dB

@Frequency 2.00e+9 Hz
CHO-TM-TP08
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Shielding Effectiveness >= 80 dB

@Frequency 1.00e+10 Hz
>= 80 dB

@Frequency 1.00e+10 Hz
CHO-TM-TP08
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..
Shielding Effectiveness 80 dB

@Thickness 1.80 mm,
Frequency 8.00e+8 - 1.80e+10 Hz
80 dB

@Thickness 0.0709 in,
Frequency 8.00e+8 - 1.80e+10 Hz
IEEE 299
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding
PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec..
Shielding Effectiveness 80 dB

@Frequency 1.00e+9 Hz
80 dB

@Frequency 1.00e+9 Hz
1mm x 6mm
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket
Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t..
Shielding Effectiveness 80 dB

@Frequency 1.00e+9 Hz
80 dB

@Frequency 1.00e+9 Hz
2mm x 6mm
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket
Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t..
Shielding Effectiveness 80 dB

@Frequency 100000 Hz
80 dB

@Frequency 100000 Hz
H-Field
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer
Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing...
Shielding Effectiveness 80 dB

@Frequency 1.00e+9 Hz
80 dB

@Frequency 1.00e+9 Hz
Plane Wave
Parker Chomerics Tecknit Teckshield®-F 145 OPI 0.0022" Diameter Wire, High Performance EMC Window
Description: TECKSHIELD-F high-performance fully laminated flat windows are specially designed to provide optimum optical transmission and EMI shielding in severe interference environments. TECKSHIE..
Shielding Effectiveness >= 80 dB

@Frequency 1.00e+10 Hz
>= 80 dB

@Frequency 1.00e+10 Hz
Plane Wave; CHO-TM-TP08
Parker Chomerics CHO-SEAL 1310 Conductive Elastomer
Moderate performance in non-corrosive environments, no corrosion or fluid resistance; material of choice for small, delicate injection-molded parts or large dimension extrusionsMolded onlyRoHS Compl..
Shielding Effectiveness 80 dB

@Frequency 1.00e+10 Hz
80 dB

@Frequency 1.00e+10 Hz
CHO-TM-TP08
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Shielding Effectiveness 80 dB

@Frequency 1.00e+10 Hz
80 dB

@Frequency 1.00e+10 Hz
CHO-TM-TP08
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Shielding Effectiveness 80 dB

@Frequency 1.00e+10 Hz
80 dB

@Frequency 1.00e+10 Hz
CHO-TM-TP08
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Shielding Effectiveness 80 dB

@Frequency 1.00e+10 Hz
80 dB

@Frequency 1.00e+10 Hz
CHO-TM-TP08
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Shielding Effectiveness >= 80 dB

@Frequency 1.00e+8 Hz
>= 80 dB

@Frequency 1.00e+8 Hz
E-Field; Method 1, CHO-TM-TP08
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer
Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics
Shielding Effectiveness >= 80 dB

@Frequency 5.00e+8 Hz
>= 80 dB

@Frequency 5.00e+8 Hz
E-Field; Method 1, CHO-TM-TP08
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer
Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics
Shielding Effectiveness 80 dB

@Frequency 1.00e+8 Hz
80 dB

@Frequency 1.00e+8 Hz
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding
Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding..
Shielding Effectiveness 80 dB

@Frequency 1.00e+10 Hz
80 dB

@Frequency 1.00e+10 Hz
CHO-TM-TP08
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..