Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 79 dB @Frequency 200000 Hz |
79 dB @Frequency 200000 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology ECF-J Silver Aluminum Loaded Fluorosilicone P & P Technology material reference ECF-J is a fluorosilicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical pro.. |
|||
Shielding Effectiveness | 79 dB @Frequency 200000 Hz |
79 dB @Frequency 200000 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-J Silver Aluminum Loaded Silicone P & P Technology material reference EC-J is a silicone elastomer with a Silver/Aluminum conductive filler. The material is specially compounded to offer excellent physical and electrical properties.. |
|||
Shielding Effectiveness | 79 dB @Frequency 1.00e+9 Hz |
79 dB @Frequency 1.00e+9 Hz |
5mm x 5mm |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Shielding Effectiveness | 79 dB @Frequency 2.00e+7 Hz |
79 dB @Frequency 2.00e+7 Hz |
|
Parker Chomerics SOFT-SHIELD® 1000 Low Closure Force, Foam Core EMI Gasket Description: Easy-to-install SOFT-SHIELD® 1000 Series gaskets are specially designed for shielding commercial electronic enclosures with tight space constraints or low closure force requirements. T.. |
|||
Shielding Effectiveness | 79 dB @Frequency 1.00e+8 Hz |
79 dB @Frequency 1.00e+8 Hz |
|
Parker Chomerics SOFT-SHIELD® 1000 Low Closure Force, Foam Core EMI Gasket Description: Easy-to-install SOFT-SHIELD® 1000 Series gaskets are specially designed for shielding commercial electronic enclosures with tight space constraints or low closure force requirements. T.. |