Polymer Property : Shielding Effectiveness = 73 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 73 dB

@Frequency 1.00e+8 Hz
73 dB

@Frequency 1.00e+8 Hz
With 360° ground termination
Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield
Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em..
Shielding Effectiveness 73 dB

@Frequency 2.00e+8 Hz
73 dB

@Frequency 2.00e+8 Hz
14" x 14" open aperture; MIL-STD-285; CHO-TM-TPO8
Parker Chomerics WIN-SHIELD™ Elite EMI Shielded Window
Description: Shielded Windows WIN-SHIELD™ EMI shielded windows provide exceptional optical performance without sacrificing EMI shielding. This new generation of shielded windows is designed specif..
Shielding Effectiveness 73 dB

@Frequency 1.00e+10 Hz
73 dB

@Frequency 1.00e+10 Hz
Parker Chomerics CHO-SHIELD® 2040 Silver-Filled Acrylic Coating for EMI Shielding
Description: CHO-SHIELD® 2040 is an electrically conductive, one-component silver filled acrylic coating that is specially formulated for application on plastic to provide premium EMI/RFI shielding..
Shielding Effectiveness 73 dB

@Frequency 1.00e+7 Hz
73 dB

@Frequency 1.00e+7 Hz
E-Field
Parker Chomerics Tecknit SC-Consil® 861 Carbon-Filled Silicone Elastomer
Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows..