Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 5.0 dB @Frequency 1.00e+10 Hz |
5.0 dB @Frequency 1.00e+10 Hz |
1/8 thickness |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Shielding Effectiveness | 5.0 dB @Frequency 4.00e+8 Hz |
5.0 dB @Frequency 4.00e+8 Hz |
With wire ground termination |
Parker Chomerics CHO-JAC CJ-021 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | 5.0 dB @Frequency 9.00e+8 Hz |
5.0 dB @Frequency 9.00e+8 Hz |
With wire ground termination |
Parker Chomerics CHO-JAC CJ-021 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | 5.0 dB @Frequency 1.00e+8 Hz |
5.0 dB @Frequency 1.00e+8 Hz |
With wire ground termination |
Parker Chomerics CHO-JAC CJ-021 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | 5.0 dB @Frequency 400 Hz |
5.0 dB @Frequency 400 Hz |
|
Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | 5.0 dB @Frequency 100 Hz |
5.0 dB @Frequency 100 Hz |
|
Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated em.. |
|||
Shielding Effectiveness | 5.0 dB @Frequency 4.00e+8 Hz |
5.0 dB @Frequency 4.00e+8 Hz |
Jacketing terminated with wires only |
Parker Chomerics CHO-JAC® CJ-022 Flat Cable EMI Shield Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight .. |
|||
Shielding Effectiveness | 5.0 dB @Frequency 4.00e+8 Hz |
5.0 dB @Frequency 4.00e+8 Hz |
Jacketing terminated with wires only |
Parker Chomerics CHO-JAC® CJ-021 Flat Cable EMI Shield Description: CHO-JAC shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into EMC compliance at an attractive cost. It is lightweight .. |